ACI 225.1T-20

ACI 225.1T-20 Removal of Optional Alkali Limit in Standard Specifications for Portland Cement

standard by American Concrete Institute, 11/01/2020

More details

Reduced price!
M00004397
New product
Limited time offer:

$24.30

$54.00

-55%

In stock

- +

Add to compare

 
More info

Full Description

Alkali-silica reactivity (ASR) is a potentially deleterious expansive reaction between alkalies in the pore solution of concrete and certain reactive aggregates. When ASR was first identified as a distress mechanism in the 1940s, cements with equivalent alkali contents below 0.60 percent by mass were shown to reduce the risk of this reaction. Subsequent research has shown that limiting the cement alkali content to 0.60 percent is not always sufficient to control deleterious ASR with every aggregate nor in all concrete mixtures. It is now well accepted that the reactivity of the aggregate and the amount of alkalies available in the concrete are more important in predicting deleterious ASR than cement alkali content alone.

 
Custom tab

This is a custom block edited from admin panel.You can insert any content here.

30 other products in the same category:

Compare 0

No products

To be determined Shipping
$0.00 Total

Check out