This method is intended to define the continuous upper temperature resistance (CUTR) of thermoplastic elastomers and thermoset rubber with durometer hardness =90 Shore A, to oxidation or other degradation when exposed solely to hot air for an extended period of timeThis method established the upper thermal aging limits of commercially available compounds as measured at 23 \mDC by retention of at least 50% original elongation and tensile at break after 1008 h of heat aging. This method does not take into account nor measure the effects of stress, environment, or temperature variations on the thermal aging characteristics of the materials tested.This method may involve hazardous materials, operations, and equipment. This SAE Standard does not address the safety problems associated with its use. It is the responsibility of the user of this document to consult and establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.This test method is based on SI units.
Product Details
Published: 09/21/2010 File Size: 1 file , 31 KB
Custom tab
This is a custom block edited from admin panel.You can insert any content here.